A quotation reads "aluminium alloy profile" and rarely names the alloy. But 6063 and 6061 are different materials: one extrudes beautifully, the other is stronger. Use 6063 for the uprights of a columbarium and they will not necessarily fail — there is simply not enough safety margin.

6063 is a classic extrusion alloy: 0.45%–0.9% magnesium, 0.2%–0.6% silicon, low impurities, good ductility. Its great advantage is that complex sections come out in one pass — door frames, trim, grooved uprights. In 6063 these shapes have high yield and good surface quality.
Mechanically, 6063-T5 runs about 170 MPa tensile and 130 MPa yield. For door frames, trim and non-load-bearing surrounds that is more than enough.
Anodising is another 6063 strength: the oxide layer is even and the colour stable, and the champagne and titanium grey families are almost all 6063.
6061 adds copper (0.15%–0.4%) to the magnesium-silicon system and can be heat-treated to T6. Tensile strength exceeds 260 MPa and yield 240 MPa — roughly 80% above 6063.
It machines well and suits connectors and load nodes. But it is harder to extrude: complex sections tend to crack, so in columbarium profiles 6061 is used for simple sections — square tube, rectangular tube, angle brackets.
It costs 30%–50% more than 6063, depending on section and temper.
Uprights. The vertical load of the whole rack concentrates here. In a four-hundred-niche hall one upright carries eight to twelve tiers Use 6061-T6 and the safety margin is adequate.
Load-bearing beams. Beams spanning more than 900 mm should be 6061. 6063 visibly sags over a long span.
Connection brackets. Load concentrates here; 6061 is more reliable.
Conversely, door frames, door surrounds, trim and light channels are fine — indeed better — in 6063, because their shapes are complex and 6061 cannot be extruded into them.

6061-T6 and 6061-T4 are not the same thing. T6 is solution-treated then artificially aged, giving maximum strength; T4 is naturally aged, lower strength but better ductility Specifying 6061 without a temper specifies nothing.
6063 is usually T5 (air-cooled after extrusion then aged) sometimes T6. For niche door frames, T5 is enough.
A purchase contract should state "alloy plus temper", for example "6061-T6" or "6063-T5". Write only "6061" and the supplier can deliver T4 without breach.
Ask for the mill certificate. The only reliable method. A proper manufacturer has a composition report and a mechanical property report for every batch.
Look at the surface. Anodised 6063 is even in tone and bright; 6061 is duller and more prone to colour variation. This is experience, not evidence.
Look at the section. 6061 has a finer grain structure and a brighter machined face. It takes experience.
Weigh it. 6061 is marginally denser (2.70 against 2.69 g/cm³) — too close to distinguish in practice.
So do not expect to identify the alloy on site Write it into the contract and require the warranty certificate to travel with the goods.
Q: Is 6063 really unsuitable for uprights?
A: It is acceptable at low tier counts and short spans if the wall is thickened. Above eight tiers or beyond a 900 mm span, use 6061-T6.
Q: Is imported profile always better than domestic?
A: No. With the right alloy and temper, domestic is entirely adequate. Failures in columbaria are mostly not material problems but wall thickness and connection problems.
Q: Can everything be 6061?
A: No. 6061 extrudes complex sections poorly, so door frame shapes cannot be produced from it, and forcing it doubles the cost. The sensible pairing is 6063 for form, 6061 for load.

The alloy of a columbarium profile is a parameter that only means something if it is written into the contract. 6063 handles shape and surface, 6061 handles load and nodes, and the combination is what makes a sound structure. The vaguer a quotation is, the more it deserves to be questioned to the end — the words "aluminium alloy" on their own explain nothing.