Once a niche door is shut, nobody stares at the gap running around it, yet that gap decides three things: whether dust gets in, whether the door rubs its paint off, and whether the door still closes in ten years The number was not picked at random — 2 to 3 mm is the only band left after several constraints have squeezed it.

A niche door hangs on hinges from the frame, and there must be clearance between frame and panel or the two will scrape as it swings. That clearance is mechanically necessary, and it is also a route — air, dust and insects all come through it. A columbarium door gap simply accepts both facts at once.
Gap width is roughly linear with dust ingress. At 2 mm, about 0.2 mm of dust accumulates on the inside face in a year; at 4 mm the accumulation more than doubles, and it settles on top of the urn. The hardest thing to clean inside a niche is the film of dust on the urn's lid, because it sits directly in line with the gap.
So the gap should be small — but small has a floor.
The lower bound comes from thermal expansion and coating thickness Niche panels are mostly 0.5–0.8 mm galvanised or 1.0 mm aluminium; at 400 mm width, a 30°C swing produces about 0.3 mm of linear expansion. Powder coating adds 60–80 microns per face, so 0.15 mm across two faces. Add the frame's own fabrication tolerance of ±0.5 mm and the total is already close to 1 mm.
Leave only 1 mm and the door binds once the plum-rain humidity arrives and the coating swells slightly; in the dry season it goes loose again. After a few cycles the paint at the gap edge goes first. A niche door is opened only a few times a year, and precisely because it is rarely opened, that binding is often not discovered until the next visit.
The upper bound comes from appearance and sealing. Beyond 3 mm the gap reads as a black line from the front and the whole row looks crude. And above 3 mm you need a seal to keep dust out, which is another operation.
So 2–3 mm is the narrow band between not rubbing and not ingesting dust. On a properly built columbarium door the gap should be equal on all four sides, within 0.5 mm. That single check says more about workmanship than any hardware brand.
Measure the gap on site and find it wide at the top and narrow at the bottom, and eight times out of ten the panel was not cut crooked — the frame is twisted. Thin-sheet frames twist easily in transport and installation, and once fitted the diagonals are unequal, so the gap is naturally wider at one end.
The test is simple: measure both diagonals of the frame. A difference over 2 mm means the frame is twisted. Adjusting hinges will not fix it; the frame has to be re-squared, or packed at the hinge side to force it level — and that is cosmetic, because the hinges will work loose within two years.
The second pattern is a gap that widens steadily from left to right along a row. That is upright plumb: if each upright is more than 1.5 mm out per metre, by the dozen position the gap is visibly skewed.
The third is a single door whose gap varies and which clicks as it swings. That is either hinge pins out of alignment or a wavy edge on the panel from shearing without levelling. Hold a straightedge against the panel edge and the high spot is where the gap is forced open.

Bare gap: under 2 mm, no seal at all. Suits a climate-controlled hall with central air, and is how most columbarium niches leave the factory. Minimal and durable; it will not stop fine dust.
Applied strip: 3–5 mm self-adhesive brush or silicone strip on the inside of the frame, compressing to 1–1.5 mm. Suits a 2.5–3 mm gap. Stick it to the frame, not the panel — on the panel it gets pulled off every time the door opens.
Extruded groove: the frame profile itself carries a groove with an EPDM gasket. The most durable option in a columbarium: the gasket is replaceable and the groove does not fail. The cost is a dedicated profile die, which puts it a grade higher.
A feeler gauge is all you need. For handover, the gauge is more reliable than the eye: take the midpoint and both ends of each of the four sides — six positions — and record the thickest blade that will enter. If the spread across those six readings exceeds 1 mm, the door is badly assembled.
Then one more action: push the door gently to just short of closed and let go. A sound door will pull itself home over the last 5 mm on the magnet or its own weight without springing back. Springing back means the hinges are preloaded and the gap has been forced; it will loosen with use.
Finally run a finger along the inside of the gap. If burrs are clearly felt, the panel was sheared without deburring — that gap will only widen, because the burr cuts a groove in the opposing face with every cycle.
Q: Can a 4 mm gap be rescued with a seal?
A: It stops dust but not the look. Even with a strip, a 4 mm gap still reads as a dark band from the front. That door is a candidate for replacement, not for a strip.
Q: Why is the gap wider at the top than the bottom on some doors?
A: Measure the frame diagonals first. Over 2 mm difference means a twisted frame, not a panel problem. Seven out of ten columbarium gap complaints come from the frame.
Q: If the gap is too small, will the door fail to open?
A: Not immediately, but eventually. Coating swelling, hinge settlement and dust accumulation add up, and a 1 mm gap becomes zero in three to five years. For a door that is rarely opened, 2.5 mm is the safer choice.

The niche door gap is craft compressed into a 2–3 mm band. Under 2 it rubs, over 3 it soils, and uneven means the frame. You do not need to inspect the lobby to judge a columbarium: open one door at random and see whether the gap is the same width on all four sides. Quality in a columbarium hides in exactly these details that nobody photographs.